Rule of thumb for drying properly stacked and stickered rough sawn timber was always 1" of thickness per year. Obviously there are many variables that influence the actual drying time including...
Type: Posts; User: Shamus
Rule of thumb for drying properly stacked and stickered rough sawn timber was always 1" of thickness per year. Obviously there are many variables that influence the actual drying time including...