Buy one of these, don't bother with adding the stainless steel media, add two tea spoons of powdered citric acid and a squirt of your favorite dish washing liquid with hot water. Set the time for two hours and bling bling! Does around 500 .223 cases per batch.
I've had a bit of a play around with differing amounts of citric acid hydrate, and the sweet spot seems to be 1/4 teaspoon in 4l of water. Any more than that doesn't seem to do them any shinier.